+86 0917-3512210
Main parameters of cr20ni80
Executive standard GB/T1234-2012
The chemical composition is:
C ≤ 0.08%;
Mn ≤ 0.6%;
P ≤ 0.02%;
S ≤ 0.015%;
Si: 0.75-1.60%;
Cr: 2.0-23.0%;
Ni: Margin.
Fe ≤ 1.0%
Al ≤ 0.5%
The maximum operating temperature of the component is 1200 ℃
Fast lifespan: not less than 80h
Melting point 1400 ℃
Density 8.4 g/cubic centimeter